Metso Corporate Newsroom News 2011 Outotec launches a new partial roasting process to purify contaminated copper and gold concentrates
Press release December 27, 2011

Outotec launches a new partial roasting process to purify contaminated copper and gold concentrates

OUTOTEC OYJ PRESS RELEASE   DECEMBER 27, 2011 1:00 PM

Outotec launches a new partial roasting process to purify contaminated copper and gold concentrates Outotec has developed a two-stage partial roasting process to remove impurities - such as arsenic, antimony and carbon - from copper and gold concentrates as a pre-treatment to actual extraction processes.

Outotec has also established a new continuous pilot plant at the company's research center in Frankfurt, Germany to test customers' concentrates with the new process. During the tests it is possible to collect reliable and necessary data for industrial process scale-up.

"This new process complements our portfolio of sustainable technologies for the minerals and metals industry. With Outotec roasting technology the harmful elements can be removed in environmentally sustainable way. We are currently building the world's largest arsenic-removing roasting furnace at Codelco's Mina Ministro Hales mine in Chile, where the new partial roasting process will be used. More than 90 percent of the arsenic contained in the concentrate can be removed to produce clean copper calcine", says Outotec CEO Pertti Korhonen.

Outotec® Partial Roasting Process
Depending on concentrate composition and plant capacity, the process can either be run in a stationary fluidized bed or in a circulating fluidized bed.

The partial roasting process for copper concentrates is a single-stage roasting process. The impurities are volatilized and the process produces calcine, which is rich in copper sulfide but has a low impurity content. The calcine is mixed and can be further processed in copper smelters. The partial roasting process is also combined with post-combustion of process gas to convert all volatile compounds into oxides.

The roasting process for refractory gold concentrates contaminated with arsenic and carbon is a two-stage process. Arsenic is removed in the first roasting stage while carbon and remaining sulfur are removed in the second stage. All sulfur, iron and carbon are fully oxidized in the process and calcine suitable for actual gold leaching is produced.  

For further information please contact:

OUTOTEC

Kari Knuutila, Chief Technology Officer
Tel. +358 20 529 2009, mobile +358 40 779 9566


Eila Paatela, Director - Corporate Communications
Tel. +358 20 529 2004, mobile +358 400 817198

Emails: firstname.lastname@outotec.com

DISTRIBUTION:
Main media
www.outotec.com